Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the wordpress-seo domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /var/www/html/wp-includes/functions.php on line 6260 Non-Tacky Daily Wear Moisturizer - Happi
Skin Care

Non-Tacky Daily Wear Moisturizer

Non-Tacky Daily Wear Moisturizer
Ingredients
%

Phase A

  • Deionized water
  • 61.15
  • Glycerin (99.7% FCC Grade) (Archer Daniels Midland)
  • 7.00
  • 1,3-Butanediol (Alfa Aesar) (Butylene glycol)
  • 4.00
  • Propylene Glycol (Sigma-Aldrich)
  • 2.00
  • Euxyl PE 9010 (Schülke & Mayr) (Phenoxyethanol (and) ethylhexylglycerin)
  • 0.80
  • Structure CEL 4400 E rheology modifier (AkzoNobel Personal Care) (Hydroxyethyl ethylcellulose)
  • 0.15

Phase B

  • Arlacel 165 (Croda Inc) (Glyceryl stearate (and) PEG-100 stearate)
  • 2.00
  • Lipovol A (Lipo Chemicals) (Persea gratissima (avocado) oil)
  • 3.00
  • Dermol IPM (Alzo Inc) (Isopropyl myristate)
  • 5.00
  • Floramac Macadamia Oil - Refined (Floratech) (Macadamia integrifolia seed oil)
  • 3.00
  • Dow Corn 200 Fluid (5 CST) (Dow Corning) (Dimethicone)
  • 1.00
  • Lipovol Sun (Lipo Chemicals) (Helianthus annuus (sunflower) seed oil)
  • 3.00

Phase C

  • Carbopol 940 (Lubrizol Advanced Material) (Carbomer)
  • 0.20

Phase D

  • Triethanolamine-99% (Dow Chemical)
  • 0.30
  • Deionized water
  • 1.00

Phase E

  • Dermacryl E (45% active) polymer (AkzoNobel Personal Care) (Styrene/acrylates copolymer)
  • 4.40

Phase F

  • Dry-Flo PC starch (AkzoNobel Personal Care) (Aluminum starch octenylsuccinate)
  • 2.00

Procedure

Phase A: In the main kettle, add everything but the Structure CEL 4400 E rheology modifier and mix under the homogenizer while heating to 75-80°C. Sprinkle in the Structure CEL 4400 E rheology modifier under moderate speed to ensure uniform hydration. Phase B: In a side kettle, add all ingredients and heat to 75-80°C under moderate propeller mixing. Once Phase A and B reach temperatures within 5 degrees of each other, add Phase B into A slowly with moderate speed homogenization. Mix for 10 minutes at 75-80°C. Then begin cooling the batch to 60°C, under low homogenization. When the batch has reached 60°C, sprinkle in Carbopol 940 and homogenize at 4000 rpm for 10 minutes until hydrated. Pre-mix Phase D and slowly add to the batch. Homogenize for 5 minutes or until homogeneous. Add Phase E and mix for another 5 minutes or until homogeneous. Cool batch to 45°C. At 45°C, sprinkle in Phase F and homogenize into the batch at low speed for 10 minutes or until uniform. Adjust the pH to 6.9-7.4. Switch the batch to a sweep blade at the lowest mixing speed (~ 20 rpm) and cool completely to room temperature. Drop the batch.

Properties

Color—White; Appearance—Opaque; pH—6.8-7.4; Viscosity—4400-10700 cps RVDV Spindle C, 10 rpm, 25°C.

More Information

AkzoNobel Surface Chemistry Personal Care 888-331-6212 Fax: 908-707-3664 Email: personalcare.usa@akzonobel.com Website: www.akzonobel.com/PersonalCare